Germany KIWOPRINT TC2500/1
Solvent-based pressure sensitive adhesive
KIWO TC-2500/1 is a high quality, transparent pressure sensitive adhesive for paper, cardboard, hard PVC, glass, iron, industrial foam cotton and polycarbonate (PC), polyester (PET), polyethylene Film sheets of (PE) and polypropylene (PP). In addition, dry pattern printing and wet transfer printing are also applicable.
Bonding with TC-2500/1 requires a bond, which is generally difficult or impossible to remove.
The coated TC-2500/1, if properly stored in dry, dark and cool and covered with silicon paper, can be stored for at least one year without reducing its cohesive force.
Generally coated TC-2500/1 has sufficient UV resistance. If there is a possibility of direct sunlight, please test first. "KIWO" TC-2500/1 is an aqueous solution resistant to water, acid and alkali, and most mineral oils.
Use
KIWOPRINT TC-2500/1 can be applied by brush, roller or screen printing. When screen printing is used, it is necessary to use a solvent-resistant emulsion such as AZOCOLPOLY-PLUSS, and the mesh is between 40-100 lines/cm. If a 51-line 7 cm screen is printed on the polyester sheet, the spread of the pressure sensitive adhesive is about 40 g/m2.
The coated pressure sensitive adhesive can be dried at room temperature or by a channel dryer. For processing, the pressure sensitive adhesive should be completely dry and transparent before it can be covered with silicon paper.
Before making any production, please test the glue for each combination part such as: printing materials, inks, liners, bonds, etc. is suitable. Special attention should be paid to whether the materials such as the combination parts are suitable for long-term compatibility. It is also necessary to look at the influence of the gasket material and the structure or roughness of the substrate. Silicon-based release, plastic surface migration, etc. should be noted.
Drying time:
The drying time depends on the amount of pressure sensitive adhesive to be dried, the material to be printed, the drying temperature and the amount of air flow.
Guide value (undried pressure sensitive adhesive film layer is 90μm thick)
--- at 20 ° C for about 20 minutes
--- at 70 ° C for about 1 minute
Pilot projects | test results |
Sticky value | about1000-1200g(Polyken Tack-Tester) |
Peel strength | 19.6 + 2.5 N/inch (2.0 + 0.25 kp/inch), measured with ASTM BE-T-EX peel tensometer. The attachment site is 2.5×250px, and the undried pressure-sensitive adhesive film layer is 90μm thick. |
Heat resistance | -20 ° C to 80 ° C (attachment portion 10 × 62.5 px, undried pressure-sensitive adhesive film layer is 90 μm thick, polyester sheet adhered to the iron sheet, load weight 30 g). |
ingredient | Latex composition |
color | Light yellow, dry and transparent |
Viscosity | about2750mPas(Rheomat STV, measuring system C11,20℃) |
Density | about0.92g/cm3 |
Solid content | about49% |
Flash point | about25℃ |
Only the fully dry pressure sensitive film layer will give the highest bond value.
Health hazards / environmental protection When operating with KIWOPRINT TC-2500/1, adequate air circulation should be allowed in the workplace. For more details, please consult MSDS.
Store for 12 months (at 20-25 ° C and tightly closed in the original container).
Packing: 4.5KG / barrel
ShenZehn Varmia Technology Co.,Ltd
Address: Room 901, Building A, Exhibition Center, E-Commerce Building, Taojindi, Tenglong Road, Longhua District, Shenzhen
Tel: 0755-27659820
Fax: 0755-27659830
Mobile: 13302956659 (Mr.liu)
Email: hmy-tech@163.com
Website: www.szhmy.net
ShenZehn Varmia Technology Co.,Ltd(Pingshan Branch)
Address: Building A, Dawan Culture Plaza, No. 4128 Dongcheng Ring Road, Mawei Street, Pingshan District, Shenzhen
Tel: 0755-27659866
Fax: 0755-27659830
Mobile: 13823780855 (Mr.Wang)
Email: yxyang@hmy varmia.com
Copyright @ 2018 ShenZehn Varmia Technology Co.,Ltd Te:0755-27659820 Fax:0755-27659830
Address: Building A, Dawan Culture Plaza, No. 4128 Dongcheng Ring Road, Mawei Street, Pingshan District, Shenzhen Mailbox:hmy-tech@163.com